MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Trinseo CALIBRE™ MEGARAD™ 2091-15 Polycarbonate Resin
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Gamma Radiation Resistant

Material Notes: CALIBRE™ MEGARAD 2091 Polycarbonate resins designed for single use medical devices (SUDs) that require gamma and electron-beam irradiation and an accelerated schedule for delivery of post-radiated products to customers – potentially 10-21 days sooner than currently available radiation-stabilized polycarbonate resins, depending on irradiation conditions. In addition, the resins are meant for applications that require a more water white appearance rather than the traditional purple tinted resin used to compensate for these sterilization methods. CALIBRE™ MEGARAD 2091-15 Polycarbonate Resin has undergone biocompatibility testing based on ISO 10993 standards (Biological Evaluation of Medical Devices) and is suitable for use in approved medical applications.

Main Characteristics:

  • Improved Color Compensation
  • Mold Release
  • Tested under ISO 10993
Applications:
  • Medical applications

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccASTM D792
Water Absorption 0.15 %
@Time 86400 sec
ISO 62
Moisture Absorption at Equilibrium 0.32 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 in/inASTM D955
Melt Flow 15 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 118ASTM D785
Tensile Strength at Break 68.0 MPaISO 527-2/50
 68.3 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 62.0 MPaISO 527-2/50
 62.1 MPa50 mm/min; ASTM D638
Elongation at Break 150 %50 mm/min; ASTM D638
 150 %ISO 527-2/50
Elongation at Yield 6.0 %50 mm/min; ASTM D638
 6.0 %ISO 527-2/50
Tensile Modulus 2300 MPa50 mm/min; ASTM D638
 2300 MPaISO 527-2/50
Flexural Strength 96.5 MPaMethod I (3 point load), 2.0 mm/min; ASTM D790
 98.0 MPa2.0 mm/min, 3 points; ISO 178
Izod Impact, Notched 378 J/mASTM D256
Izod Impact, Notched (ISO) 75.0 kJ/m²ISO 180/A
Izod Impact, Unnotched (ISO) NBISO 180
Tensile Impact Strength 378 kJ/m²ASTM D1822
Dart Drop, Total Energy 81.3 J3.39 m/sec; ASTM D3763
Abrasion 45[%], Taber; ASTM D1044

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTRINS9041 / 197541

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.