Temper: As Continuous Cast Casting Characteristics: High – Casting Yield, Fluidity; Medium –Gassing; Low - Drossing, Effect of Section Size, Shrinkage in Solidification Fabrication Properties: Good Suitability – Soldering; Poor Suitability – Brazing Typical uses: High Speed Bearings for Light Loads; High Speed, Light to Medium Pressure Bushings; Railroad Applications; Soft Bushings; Soft Metal Applications Applicable Specifications: As Centrifugal Cast – Castings SAE J461, Castings SAE J462, Castings ASTM B271/B271M; As Continuous Cast – Castings SAE J462, Castings SAE J461, Castings ASTM B505/B505M; As Sand Cast – MILITARY MIL-C-22229, Castings ASTM B763/B763M, Castings SAE J462, ASTM B66, Castings SAE J461, Castings ASTM B584; Ingot - ASTM B30 |