MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lanxess PUROLAN® IOC Trimethylpentane Solvent
Categories: Fluid; Solvent

Material Notes: PUROLAN® IOC is a colorless liquid with low odor intensity. It is volatile and evaporates rapidly. PUROLAN® IOC is an excellent solvent where quick drying without residue of the solvent is desired. Compared to other volatile solvents skin irritation is low.

INCI: Isooctane

CAS No.: 540-84-1

EINECS No.: 208-759-1

Application:

    Volatile solvent
  • Replacement for more irritating solvents in removers and cleansers
Advantages:
  • low skin irritation compared to other volatile solvents
  • colorless
  • good compatibility with other ingredients
  • highly stable

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.690 g/cc
@Temperature 20.0 °C
 0.700 g/cc
@Temperature 15.0 °C
Vapor Pressure 0.0600 bar
 
Thermal PropertiesOriginal ValueComments
Boiling Point 98.0 °Crange start
 100 °C5% by vol
 101 °C95% by vol
 102 °Crange end
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.392nD20
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 0.0050 %<50 mg/kg
Sulfur, S <= 0.00010 %<1 mg/kg
 
Descriptive Properties
Content<0.01 mg/gNeutralization number (as KOH)
 <1 mg/100mlEvaporation residue
 <1 mg/kgAromatics
 <1 mg/kgPeroxides (as H2O2)
 <10 mg Br2/100gBromine index
 <2 mg/kgCarbonyls
 >90%2,2,4-trimethylpentane
 >98%Sum of C8 hydrocarbons

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLANY8130 / 208523

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.