MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Guang Dong LH-POM NC89 Antistatic POM
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Application Field: Suitable for extruding plastic sheets and rods

Feature: Good toughness, high impact, high strength, strong rigidity, rub resistance, good thermal stability and creep resistance

Grade: Extrusion

Color: Natural white, color matching service available

Information provided by GuangDong LuHua New Material Technology Holding Co

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 - 1.50 g/cc1.30 - 1.50 g/ccGB1033-86
Melt Flow 13 g/10 min
@Load 2.16 kg,
Temperature 220 °C
13 g/10 min
@Load 4.76 lb,
Temperature 428 °F
GB/T3682
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 86.286.2GB3942-88
Tensile Strength 40.0 MPa5800 psiGB/T1040-1992
Flexural Strength 30.0 MPa4350 psiGB/T9341-2008
Flexural Modulus 0.750 GPa109 ksiGB/T9341-2008
Tensile Impact Strength 16.0 kJ/m²7.61 ft-lb/in²GB/T1843-80
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+8 - 1.00e+9 ohm1.00e+8 - 1.00e+9 ohmGB/T1410
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 164.83 °C328.69 °FGB1633-79
Heat Distortion Temperature 72.2 °C162 °FGB/T1634.2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGDON005 / 283953

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.