MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
ChevronTexaco 100R Neutral Oil
Categories: Fluid; Lubricant

Material Notes: Features

Chevron Neutral Oils are all-hydroprocessed, highly refined API Group II paraffinic base stocks. Their extremely low sulfur, nitrogen, and aromatic content give them excellent thermal and oxidation stability.

These base oils provide excellent cold flow performance because the ISODEWAXING® catalyst and technology convert almost all of the wax in the feed into branched compounds.

Chevron Neutral Oils offer the following characteristics relative to typical Group I (solvent refined) base stocks:

  • Lower volatility and cold cranking simulator (CCS) viscosity to meet modern engine oil specifications such as ILSAC GF-3
  • Better oxidation and thermal stability
  • Lower aromatics, sulfur and nitrogen
  • Improved response to pour point depressants
  • Improved soot dispersancy in heavy duty motor oil formulations
Chevron Neutral Oils 100R, 220R, and 600R are API Group II base stocks with a typical viscosity index of 99-103.

Chevron Neutral Oil 5R is a 5 cSt Group II "plus" base stock with a typical viscosity index of 115-117. It was designed to meet the low volatility requirements of next generation (ILSAC GF-3) passenger car motor oils while maintaining API Group II status.

Applications

When combined with properly selected additives, Chevron Neutral Oils are ideal for blending a wide variety of finished products, including:

  • Passenger car motor oils
  • Heavy duty motor oils
  • Industrial engine oils
  • Tractor hydraulic fluids
  • Transmission fluids
  • Gear oils
  • Greases
  • Hydraulic oils
  • Ammonia refrigeration oils
  • Paper machine oils
  • Compressor oils
  • Process oils
  • Lubricant additives

Key Words: CPS Number: 240667; MSDS Number: 6986
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.8529 g/cc
API Gravity 34.4 °
Viscosity 1450 cP
@Temperature -25.0 °C
Cold Crank
Viscosity Measurement 98Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 104 SUS
Kinematic Viscosity at 40°C (104°F) 19.7 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 4.0 cStASTM D445
Collected Volatile Condensable Material 15 %ASTM D2887
Evaporation Loss 27 %CEC L-40-A-93
 
Thermal PropertiesOriginal ValueComments
Pour Point -12.0 °CASTM D97
Flash Point 213 °CASTM D92
 
Descriptive Properties
Aromatics, by HPLC, %<1
Carbon Type by n-d-m, % Naphthenic33
Carbon Type by n-d-m, %Aromatic<1
Carbon Type by n-d-m, %Paraffinic67
ColorL 0.5
Saturates, by HPLC, %>99
Sulfur, ppm10
Water Separability, Minutes to 0 mL emulsion15
Water, ppm39

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCHEV410 / 75025

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.