MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Kraiburg TPE THERMOLAST® H TH8PGMNTRL Thermoplastic Elastomer (HC/AD1/AP Series)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: The HC/AD1/AP series is a material solutions exclusively designed for healthcare and medical device applications in Asia Pacific. These compounds comply with ISO 10993-5 and GB/T 16886.5. They are characterized by their adhesion properties to polar thermoplastics such as PC, ABS, and PETG and are available in natural colors.

Processing Method: Injection Molding

Color / RAL DESIGN:

  • Natural
Typical applications:
  • Function and design elements
  • Soft touch for grips, switches and mats
  • Seals
  • Valves
  • Flexible Connections
  • Membranes
Material advantages:
  • Adhesion to PC, ABS, PC/ABS, ASA, SAN
  • Adhesion to PET and PETG
  • Adhesion to PS
  • Sterilizable
  • Optimized mechanical properties
  • Soft touch surface
  • Colorable
  • Free from animal ingredients

Information provided by Kraiburg TPE

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.03 g/cc0.0372 lb/in³DIN EN ISO 1183-1
Storage Temperature 15.0 - 30.0 °C59.0 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080DIN ISO 48-4
Tensile Strength 11.0 MPa1600 psi200 mm/min; DIN 53504/ISO 37
Elongation at Break 700 %700 %200 mm/min; DIN 53504/ISO 37
 
Descriptive Properties
Adhesion to ABS3.7 N/mm (A)VDI 2019 two-component injection
Adhesion to PC9.7 N/mm (B/D)VDI 2019 two-component injection
ColorNatural

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKRAIA8439 / 309103

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.