MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo STYRON A-TECH™ 1200 High-Impact Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: STYRON A-TECH™ 1200 is a newly developed, high-impact polystyrene (HIPS) reins based on patented technology. The technology platform for STYRON A-TECH™ makes it possible to eliminate the typical trade-offs among the key properties for HIPS including toughness, gloss, stiffness and processability.

Main Characteristics:

  • Unique combination of toughness and stiffness
  • Ease of processing
  • Excellent thermoforming behavior
  • Good blendability with General Purpose Polystyrene (GPPS)
  • Allows for down-gauging
Applications:
  • Form Fill Seal (FFS)
  • Pre-Forms (DFS)
  • Vending cups
Complies with:
  • Europe REGULATION (EC) 10/2011
  • FDA, 21 CFR.177.1640
  • Consult the regulations for complete details

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 g/ccISO 1183
Apparent Bulk Density 0.600 g/ccISO 60
Melt Flow 5.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 22.0 MPaISO 527-2/5
Tensile Strength, Yield 19.5 MPaISO 527-2/5
Elongation at Break 65 %Nominal; ISO 527-2/5
Tensile Modulus 750 MPaISO 527-2/1
Flexural Strength 38.0 MPaISO 178
Flexural Modulus 1950 MPaISO 178
Izod Impact, Notched (ISO) 14.0 kJ/m²ISO 180
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 100 °CISO 306/A120
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
INEOS Styrolution PS 486N HIPS
INEOS Styrolution PS 165 N/L GPPS
Americas Styrenics STYRON® 686E High Heat Crystal Polystyrene
Americas Styrenics STYRON® 678D High Heat Crystal Polystyrene
Overview of materials for Polystyrene, Transparent Grade

PTRINS9091 / 197564

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.