MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Rogers Arlon 99322B015 0.015" Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Categories: Polymer; Thermoset; Silicone; Silicone, Molded, Glass Fiber Filled

Material Notes: Static dissipating silicone

Design/Construction:

  • Interleave: 0.0025" Polyethylene
  • Side 1: Cured Silicone Rubber
  • Carrier: 0.003" PTFE coated Fiberglass

Recommended Primer: Chemlock 607

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³Silicone Property; Arlon SQA-TMS-024
Thickness 76.2 microns3.00 milCarrier; Arlon SQA-TMS-003
 381 microns15.0 milRubber; Arlon SQA-TMS-003
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2525Silicone Property; Arlon SQA-TMS-014
Tensile Strength 4.83 MPa700 psiSilicone Property; Arlon SQA-TMS-008
Elongation at Break 290 %290 %Silicone Property; Arlon SQA-TMS-008
Tear Strength 12.3 kN/m70.0 pliDie B; Silicone Property; Arlon SQA-TMS-029
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Inert 204 °C400 °F
Minimum Service Temperature, Air -56.7 °C-70.0 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 60.0 Month
@Temperature 21.1 °C
60.0 Month
@Temperature 70.0 °F
 
Descriptive Properties
ColorBlack
Total Product Weight (oz/yd2)13.4Arlon SQA-TMS-025

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PARL9823 / 148976

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.