MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

HB Fuller Körapop 125 Adhesive and sealant
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes:

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/cc
Solids Content 94 %94 %
Storage Temperature 5.00 - 25.0 °C41.0 - 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4848after 28 d; thickness of specimen = 6 mm; DIN ISO 7619-1
Tensile Strength 2.00 MPa290 psiDIN EN ISO 527
Elongation at Break 500 %500 %DIN EN ISO 527
Tensile Modulus 0.00200 GPa
@Strain 100 %
0.290 ksi
@Strain 100 %
Young’s; DIN EN ISO 527 / DIN 53 504
Shear Strength 1.80 MPa261 psiLap, aluminum/aluminum; DIN EN 1465
Tear Strength 9.00 kN/m51.4 pliISO 34-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+10 ohm-cm>= 1.00e+10 ohm-cmKö-test method 100262
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 90.0 °C194 °F
 120 °C
@Time 216000 sec
248 °F
@Time 60.0 hour
Short-term
Minimum Service Temperature, Air -60.0 °C-76.0 °F
Glass Transition Temp, Tg -45.0 °C-49.0 °FDIN EN ISO 6721-1
 
Processing PropertiesMetricEnglishComments
Cure Time 45.0 min0.750 hourSkin Formation Time
 
Descriptive Properties
Colorblack, white, grey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHBFULL101 / 316892

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.