MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Encom Polymers EnPure 0816R PC, Mold Release
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: Appearance: Black, Natural or Colors

Processing Methods: Injection Molding, Profile Extrusion

Applications: Automotive, Business Equipment

Information provided by EnCom Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Maximum Moisture Content 0.0200.020
Linear Mold Shrinkage, Flow 0.060 cm/cm
@Thickness 3.20 mm
0.060 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 8.5 g/10 min
@Load 1.20 kg,
Temperature 300 °C
8.5 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 62.0 MPa8990 psiASTM D638
Elongation at Break 115 %115 %ASTM D638
Flexural Strength 83.0 MPa12000 psiASTM D790
Flexural Modulus 2.31 GPa335 ksiASTM D790
Izod Impact, Notched 8.54 J/cm16.0 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 137 °C279 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 132 °C270 °FASTM D648
Flammability, UL94 V-2
@Thickness 3.17 mm
V-2
@Thickness 0.125 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 271 - 293 °C520 - 560 °F
Middle Barrel Temperature 282 - 304 °C540 - 580 °F
Front Barrel Temperature 288 - 316 °C550 - 600 °F
Nozzle Temperature 288 - 310 °C550 - 590 °F
Melt Temperature 293 - 316 °C560 - 600 °F
Mold Temperature 71.1 - 98.9 °C160 - 210 °F
Drying Temperature 104 - 121 °C220 - 250 °F
Dry Time 4.00 hour4.00 hour
 <= 7.00 hour<= 7.00 hour
Back Pressure 0.345 - 0.689 MPa50.0 - 100 psi
Shot Size 40 - 75 %40 - 75 %
Vent Depth 0.00381 - 0.00762 cm0.00150 - 0.00300 in
Screw Speed 30 - 70 rpm30 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENCOM110 / 266124

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.