MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Covestro Makrofol® BL 2-4 820816 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: Characterization: Makrofol BL 2-4 820816 is an extrusion film based on Makrolon® polycarbonate.

Properties / Applications: Makrofol BL 2-4 820816 comprises excellent die-cutting performance combined with high light transmission and moderate light scattering properties. Typical applications are automotive instrument panels, illuminated gauges, dials and graphics, front panels and scales on radios and control consoles, and diffusors on projection screens. Makrofol BL 2-4 820816 is available in two standard thicknesses; 0.012 ” and 0.016 ” (300 microns and 400 microns). Other thicknesses are available on request. The surface combination of Makrofol BL 2-4 820816 is one side very fine matte and one side fine matte. As with any product, use of Makrofol BL 2-4 820816 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/in³ASTM D792
Water Absorption 0.35 %
@Time 86400 sec
0.35 %
@Time 24.0 hour
immersion; ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 60.0 MPa8700 psiASTM D882
Elongation at Break >= 100 %>= 100 %ASTM D882
Tensile Modulus 2.10 GPa305 ksiASTM D882
 
Thermal PropertiesMetricEnglishComments
Shrinkage  <= 0.20 %
@Temperature 130 °C,
Time 3600 sec
<= 0.20 %
@Temperature 266 °F,
Time 1.00 hour
parallel; IEC 60674-2
 <= 0.20 %
@Temperature 130 °C,
Time 3600 sec
<= 0.20 %
@Temperature 266 °F,
Time 1.00 hour
parallel; IEC 60674-2
 
Optical PropertiesMetricEnglishComments
Gloss <= 15 %<= 15 %60° reverse side; ASTM D2457
 75 %75 %60° top side; ASTM D2457
Transmission, Visible >= 80 %>= 80 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrofol® DE 1-1 000000 Polycarbonate
Covestro Makrofol® ID 4-4 Polycarbonate
Covestro Makrofol® LT 4-4 Polycarbonate
Covestro Makrofol® BL 6-2 820802 Polycarbonate
Covestro Makrofol® DE 1-4 000000 Polycarbonate

PB09864 / 92704

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.