MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Polymer Resources PC-FR-UV-10-0002-16A Polycarbonate, Flame Retardant, Medium Flow  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, PTFE Filled; Polycarbonate, Unreinforced, Flame Retardant

Material Notes: Polycarbonate, Flame Retardant, Medium Flow

Features: • Ultra High Impact Resistance • Self Extinguishing
Process: Injection Molding
Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.

Information provided by Polymer Resources Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cmASTM D955
Melt Flow 9.0 - 16 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 9000 psiASTM D638
Tensile Strength, Yield 10000 psiASTM D638
Flexural Strength 13900 psiASTM D790
Flexural Modulus 335 ksiASTM D790
Izod Impact, Notched 15.0 ft-lb/in
@Temperature 22.8 °C
ASTM D256
Gardner Impact 320 in-lbASTM D3029
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 275 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 265 °FASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 510 - 550 °F
Middle Barrel Temperature 530 - 570 °F
Front Barrel Temperature 550 - 590 °F
Melt Temperature 540 - 590 °F
Mold Temperature 160 - 200 °F
Drying Temperature 245 - 255 °F
Dry Time 3.00 - 4.00 hour

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polytetrafluoroethylene (PTFE), Carbon Fiber Filled
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
AISI Type 317L Stainless Steel, annealed tubing
AISI Type 317L Stainless Steel, annealed sheet

PPOLYQ130a / 160649

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.