MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Bethlehem Steel ASTM A678 Grade D 3/16 to 3 in. thick, steel plate  (discontinued **)
Categories: Metal; Ferrous Metal; ASTM Steel; Carbon Steel; Low Carbon Steel

Material Notes: Carbon grade for plates made to a fine grain practice. The plate is heat treated by quenching and tempering to develop the high strength levels. The steel has high notch toughness. It is used in demanding structural, industrial and machinery applications where weight reduction is important and notch toughness is a design consideration.

Information provided by Bethlehem Steel Corporation

Data published in 1997. Bethlehem Steel in no longer in business.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/ccTypical of ASTM Steel
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 190 - 228based on conversion from tensile strength
Hardness, Rockwell B 91 - 98based on conversion from tensile strength
Tensile Strength at Break 90000 - 110000 psi
Tensile Strength, Yield >= 75000 psi
Elongation at Break >= 16 %in 2", > 24" W
Bend Radius, Minimum 2.0 t≤3/4" W; ASTM A6 PARA. S14
 3.0 t>3/4 to 2" W; ASTM A6 PARA. S14
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.22 %
Copper, Cu >= 0.20 %
Iron, Fe >= 97.405 %
Manganese, Mn 1.15 - 1.5 %
Nitrogen, N 0.010 - 0.030 %
Phosphorus, P <= 0.035 %
Silicon, Si 0.15 - 0.50 %
Vanadium, V 0.040 - 0.11 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Pewter, Cold-Rolled Sheet
ASTM A606 HSLA Steel, Cold Rolled Sheet
AK Steel ZINCGRIP® FORMABLE 50K / ASTM A1008 class 1 / SAE J1392 050 XLK, Grade 50 Electrogalvanized Carbon Steel, High Strength Low Alloy Steel (HSLAS)
AK Steel ZINCGRIP® FORMABLE 50K / ASTM A1008 class 2 / SAE J1392 050 XLK, Grade 50 Electrogalvanized Carbon Steel, High Strength Low Alloy Steel (HSLAS)

NBETH063 / 15422

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.