MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Thermal Ceramics Alfibond A5 Shapes
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Alfibond A5 is the highest quality ceramic fiber insulations manufactured from inorganic binders and a blend of high purity alumina-silica fibers and polycrystalline alumina fibers used in applications where strength and temperature are very important.

Features:

  • No organic binders
  • Nominal 29 lb/ft3 (13 kg/m3) density ceramic fiber insulation
  • Non wetting to aluminum
  • Complex shape capability
  • Low thermal conductivity and heat storage
  • High resistance to thermal shock and molten aluminum attack
  • Advanced vacuum forming technology produces unique insulating products
  • Applications:

  • Ladle liners
  • Transfer launders
  • Sample ladles
  • Die casting of metals
  • Burner blocks
  • Hot face linings
  • Applications where dense ceramic fiber products are required
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 0.416 g/cc
    Loss On Ignition 6.0 - 9.0 %
     
    Mechanical PropertiesOriginal ValueComments
    Modulus of Rupture 0.250 - 0.280 ksiafter 24 hour isothermal soak
    Compressive Yield Strength 0.120 MPaafter 24 hour isothermal soak, at 5% deformation
     0.160 MPaafter 24 hour isothermal soak, at 10% deformation
     
    Thermal PropertiesOriginal ValueComments
    CTE, linear 2.80 µin/in-°F
    @Temperature 20.0 °C
    Specific Heat Capacity 0.270 BTU/lb-°F
    Thermal Conductivity 0.720 BTU-in/hr-ft²-°F
    @Temperature 538 °C
    ASTM C210
     1.01 BTU-in/hr-ft²-°F
    @Temperature 816 °C
    ASTM C210
     1.44 BTU-in/hr-ft²-°F
    @Temperature 1090 °C
    ASTM C210
    Melting Point 3200 °F
    Maximum Service Temperature, Air 2800 °F
    Shrinkage 0.10 %
    @Temperature 871 °C
     0.10 %
    @Temperature 982 °C
     0.30 %
    @Temperature 1090 °C
     0.50 %
    @Temperature 1540 °C
     0.80 %
    @Temperature 1200 °C
     0.90 %
    @Temperature 1320 °C
     1.0 %
    @Temperature 1430 °C
     
    Component Elements PropertiesOriginal ValueComments
    Al2O3 70 %
    Other <= 1.0 %
    SiO2 30 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    CTHERM198 / 2518

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.