MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Rogers Arlon 51231R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Silicone, Molded, Glass Fiber Filled

Material Notes: Design/Construction:
Interleave 1: Polyethylene
Side 1: Uncured Silicone Rubber
Substrate: Style 7628 Fiberglass
Side 2: Uncured Silicone Rubber
Interleave 2: Polyethylene

This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.28 g/cc0.0462 lb/in³Silicone Property; Arlon SQA-TMS-024
Thickness 76.2 microns3.00 milInterleave 1
 76.2 microns3.00 milInterleave 2
 152 microns6.00 milSide 1; Arlon SQA-TMS-003
 152 microns6.00 milSide 2; Arlon SQA-TMS-003
 203 microns8.00 milSubstrate; Arlon SQA-TMS-003
 508 microns20.0 milOverall; Arlon SQA-TMS-003
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8383Silicone Property; ASTM D2240
Tensile Strength 7.329 MPa1063 psiSilicone Property; ASTM D412
Elongation at Break 134 %134 %Silicone Property; ASTM D412
Tear Strength 25.2 kN/m144 pli[ppiw], Die B, Silicone Property; ASTM D624
Peel Strength 0.526 kN/m3.00 pli[ppiw], Bond Strength to 6061 aluminum (90° peel test); Arlon-SQA-TMS-011
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 232 °C450 °F
Minimum Service Temperature, Air -56.7 °C-70.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 15.0 min
@Pressure 0.345 MPa,
Temperature 177 °C
0.250 hour
@Pressure 50.0 psi,
Temperature 350 °F
Recommended Cure Cycle
Shelf Life 6.00 Month
@Temperature 7.22 °C
6.00 Month
@Temperature 45.0 °F
From date of manufacture
 
Descriptive Properties
ColorRed
 RedSubstrate
Total Product Weight (oz/yd2)21.6Arlon SQA-TMS-025

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 6069-T6, 0.5 in x 3 in. Bar, Hot Hollow Extrusion, Average Tensile Values
Aluminum 6061-T913
Aluminum 6061-T91
Aluminum 6061-T8
Aluminum 6061-T6; 6061-T651

PARL266 / 125452

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.