MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ChevronTexaco Clarity® ISO 46 Saw Guide Oil
Categories: Fluid; Lubricant

Material Notes: Features

Chevron Clarity Saw Guide Oils are designed to promote longer saw guide and saw blade life in thin kerf saw equipment, when operating in severe service and reduced cooling water modes.

Chevron Clarity Saw Guide Oils are formulated with ISOSYN® base stocks and specially selected ashless additives to reduce friction between saw and guide components in thin kerf saw equipment.

The oils lubricity performance minimizes rust and corrosion problems, while reducing friction to allow much cooler operation.

Chevron Clarity Saw Guide Oils have been formulated with effective rust inhibitors to prevent rust formation. Oiliness and EP properties provide excellent film strength for boundary lubrication and extreme pressure conditions.

Chevron Clarity Saw Guide Oils have the optimum emulsification to allow the correct mixing of oil and water and have tackiness properties to enable the lubricants to cling to saw and guide components.

Applications

Chevron Clarity Saw Guide Oils are specifically formulated to lubricate modern thin kerf sawing systems. Original Equipment Manufacturers and sawmill customers were consulted prior to product design and laboratory testing. Chevron Clarity Saw Guide Oils performance properties have been field proven to meet the severe requirements of this application.

Chevron Clarity Saw Guide Oils meet or exceed the performance requirements of most saw system manufacturers, including: CAE (Newnes, McGehee), Optimil, Salem, TMT, Ukiah, and USNR (Kockums CanCar, Schurman).

Chevron Clarity Saw Guide Oil ISO 46 is recommended for and has been used successfully in band saw mist applications.

Key Words: CPS Number: 255199; MSDS Number: 6716
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 32.4 °
Viscosity Measurement 118Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 224 SUS
Saybolt Viscosity at 210°F 50 SUS
Kinematic Viscosity at 40°C (104°F) 43.7 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 7.0 cStASTM D445
 
Thermal PropertiesOriginal ValueComments
Pour Point -33.0 °CASTM D97
Flash Point 242 °CASTM D92
 
Descriptive Properties
Rust preventative Test Procedure BPassSynthetic Sea Water

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCHEV157 / 74772

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.