MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Epoxies, Etc 20-2162 Urethane Sealant, Adhesive & Potting Compound
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: 2162 is engineered for demanding applications where flow control is necessary to limit mold leaking, seeping around cable entries and substrate wicking. This product offers outstanding durability and adhesion to a variety of substrates.

Features:

  • Outstanding environmental performance
  • Controlled flow
  • Easy mixing
  • High impact resistance
  • Available in Triggerbond® cartridges

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.01 g/cc1.01 g/ccPolyol
 1.14 g/cc1.14 g/ccIso
Viscosity 750 cP750 cPIso
 1200 cP1200 cPPolyol
Linear Mold Shrinkage 0.014 cm/cm0.014 in/in
Storage Temperature 24.0 - 30.0 °C75.2 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 45 - 55
@Temperature 25.0 °C
45 - 55
@Temperature 77.0 °F
Overnight
 45 - 55
@Temperature 60.0 °C,
Time 18000 sec
45 - 55
@Temperature 140 °F,
Time 5.00 hour
 60 - 70
@Temperature 25.0 °C,
Time 432000 sec
60 - 70
@Temperature 77.0 °F,
Time 120 hour
Tensile Strength 5.52 MPa800 psi
Elongation at Break 200 %200 %
Tear Strength 2.63 kN/m15.0 pli
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 7.20e+13 ohm-cm7.20e+13 ohm-cm
Surface Resistance >= 1.00e+14 ohm>= 1.00e+14 ohm
Dielectric Constant 3.4
@Frequency 1000 Hz
3.4
@Frequency 1000 Hz
Dielectric Strength >= 21.7 kV/mm>= 550 kV/in
Dissipation Factor 0.017
@Frequency 1000 Hz
0.017
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.300 W/m-K2.08 BTU-in/hr-ft²-°F
 
Descriptive Properties
ColorBlack
Working TimeInitial Self Leveling
 Set Time
 Workable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFEPOX085 / 316762

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.