MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Poraver 4-8 mm Expanded Glass
Categories: Ceramic; Glass

Material Notes:

Information provided by Poraver®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.152 - 0.207 g/cc0.00550 - 0.00747 lb/in³Dry loose; ASTM C9/C29M
Density 0.256 - 0.343 g/cc0.00926 - 0.0124 lb/in³ASTM C128
Water Absorption 5.0 %5.0 %by volume; ASTM C128
 20 %20 %by mass; ASTM C128
Water Absorption at Saturation <= 0.50 %<= 0.50 %
Particle Mesh Size 5.5 - 16 Mesh5.5 - 16 MeshASTM C136
pH 9.0 - 129.0 - 12
Thickness 4000 - 8000 microns157 - 315 milGrain size; ASTM C136
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 1.20 MPa174 psiEN 13055-1
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0700 W/m-K0.486 BTU-in/hr-ft²-°F
Softening Point 700 °C1290 °F
 
Component Elements PropertiesMetricEnglishComments
Loss on Ignition(%) 1.0 %1.0 %ASTM C114
 
Descriptive Properties
Colorcreamy white
Finess Modulus5.73ASTM C136

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pyrotek ISOMAG® 175 Structural Insulation Board
Du-Co Ceramics DC-187 Magnesium Oxide
Poraver 0.1-0.3 mm Expanded Glass
Goodfellow Cellophane, Rayophane Regenerated Cellulose Film
Du-Co Ceramics DC-142 Aluminum Silicate

CPOR026 / 186915

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.