MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Teknor Apex APEX® S3610-85NT Polyvinyl Chloride
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Notes: APEX S3610-85NTis a Polyvinyl Chloride Medical Extrusion Compound available in pellet form. It complies with NSF/ANSI STANDARD 61.

Availability: Asia Pacific

Uses: Hose; Sheet

Form: Pellets

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8181ASTM D2240
Tensile Strength at Break 19.0 MPa2760 psi0.2 in/min; ASTM D638
Elongation at Break 350 %350 %ASTM D638
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 190 °C
@Time >=1800 sec
374 °F
@Time >=0.500 hour
Thermal Stability; ASTM D794
 
Processing PropertiesMetricEnglishComments
Processing Temperature 155 - 165 °C311 - 329 °FCompression Zone
 160 - 170 °C320 - 338 °FMixing Zone
Feed Temperature 145 °C293 °F
Nozzle Temperature 170 - 185 °C338 - 365 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0365 / 236856

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.