MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Wynca WynPh ® FR700 Halophosphate-free Flame Retardant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Advantages:
  • Small particle size, high accumulation density, easy to blanking , easy to disperse in polymer system, etc.
  • Small particle size, high accumulation density, easy to blanking , easy to disperse in polymer system, etc.
  • Halogen-free flame retardant, low-toxic and low-smoke, safe and environmentally friendly, meets RoHS and REACH regulatory requirements.
Application and Suggestion:Halogen-free flame retardant FR700 can be combined with a variety of synergistic agents to achieve flame retardant requirements based on customer specific needs. In the field of thermoplastic elastomer (TPE, TPU, etc.). There are good physical properties and excellent flame retardancy in the modified system compounded with other synergists containing nitrogen or/and phosphorus.

Information provided by Wynca Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.50 %<= 0.50 %
Grain Size <= 10 µm<= 10 µmD50
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature >= 300 °C>= 572 °F
 
Component Elements PropertiesMetricEnglishComments
Phosphorus, P 41 - 42 %41 - 42 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWYNCA091 / 320649

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.