MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ExxonMobil 422 Mobilmet 400 Series
Categories: Fluid; Lubricant

Material Notes: Mobilmet 400 Series products are high-performance multi-purpose cutting oils. They are chlorine-free, non-staining and non-corrosive. They are designed for light to moderate duty cutting operations and they are also suitable as machine tool lubricants and for use in light duty hydraulic systems. They are formulated from high quality base oils and select additives to provide effective machining performance in a wide variety of operations of both ferrous and non-ferrous metals. The oils are light-colored and transparent so that the work area can be clearly seen at all times. The higher viscosity Mobilmet 420s are formulated to prevent the formation of oil mist in the vacinity of the machine tool. Mobilmet 400 Series fluids are resistant to foaming, even with excess splashing so that superior performance is provided in the machine tool lubrication system. With relatively low pour points and high viscosity indexes, they are not difficult to dispense in cold conditions and provide adequate film strength in hot-running machine tool bearings under load.

Mobilmet 400 Series fluids are recommended for a wide range of machining operations on all types of metals. They can be used as multi-purpose oils when a common fluid is required for machine tool lubrication and as a hydraulic fluid assuming proper viscosity selection.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.845 g/cc
@Temperature 15.0 °C
0.845 g/cc
@Temperature 59.0 °F
ASTM D1298
Viscosity Measurement 139139Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 26.6 cSt26.6 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 3.7 cSt3.7 cStASTM D445
 
Thermal PropertiesMetricEnglishComments
Pour Point -7.50 °C18.5 °FASTM D97
Flash Point 158 °C316 °FASTM D92
 
Descriptive Properties
Copper Strip Corrosion1B3 hrs @ 100°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil PP8013L1 Polypropylene Impact Copolymer
ExxonMobil PP7694E2 Impact Copolymer
ExxonMobil PP7043L1 Polypropylene Impact Copolymer
ExxonMobil PP7032KN Impact Copolymer
ExxonMobil PP5722E1 Polypropylene Copolymer

WEXXON284 / 75709

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.