MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Heligoen® Blue L 7080 Color Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: ß-phthalocyanine blue for economic formulations

Chemical Structure: Cu-phthalocyanine, beta

Physical form: Powder

Suitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, Acid curing systems, Amine curing systems, and Airdrying systems.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.61 g/cc
Specific Surface Area 63 m²/g
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 4.0 - 7.0
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 5000 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 300 °C
 
Descriptive Properties
Chemical Fastness (months)Butylacetate4-5
 Ethanol4
 HCL 2%5
 Methyl ethyl ketone3
 Mineral spirits5
 NaOH 2%5
 Solvenon™PM5
 Xylene5
ColorBlue
Fastness to Overcoating5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Inovyn 266SC Polyvinyl Chloride Pastes - filler Polymers
Blue River Coatings Wood Primer
A. Schulman POLYBLAK™ 2723Pm Premium Black Color Concentrate, 25% Carbon Black Based In HDPE
Universal Wire Works ER317L Stainless Steel Bare Wire
Allnex UCECOAT® 2501 Waterborne UV Resin

PBASG0723 / 132356

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.