MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ChevronTexaco Synthetic Automatic Transmission Fluid, Heavy Duty
Categories: Fluid; Lubricant

Material Notes: Features

Chevron Synthetic Automatic Transmission Fluid Heavy Duty is engineered to meet the performance requirements of Allison TES 295 for severe duty and extended drain intervals. It is manufactured from synthetic base oils and additives that provide oxidation and thermal stability, friction control, load-carrying ability, corrosion and wear protection. It prevents the accumulation of deposits and the formation of sludge, varnish, and foam. Chevron Synthetic Automatic Transmission Fluid Heavy Duty has excellent low temperature flow properties and enhanced protection against viscosity breakdown. Under the most severe operating conditions, this fluid:

  • maintains friction control for smooth shift action
  • retains low temperature fluidity and high temperature stability for long operating periods.
  • provides excellent antiwear protection.
  • greatly extends the time to transmission overhauls due to sludge, corrosion, wear of clutches and bands, gears and bearings, leakage past seals, and loss of frictional properties.

    Applications

    Chevron Synthetic Automatic Transmission Fluid Heavy Duty is specially engineered for heavy duty automatic truck and bus transmissions operating in extended service. It is also an excellent choice for passenger cars and light trucks requiring Ford MERCON®, MERCON V, or General Motors DEXRON®-III1, especially for those vehicles in moderate to severe service. The following examples represent some of the applications that will benefit greatly from the use of Synthetic ATF Heavy Duty versus conventional ATF: police cars, taxicabs, pickup & delivery trucks, recreational vehicles, and tow trucks.

Key Words: CPS Number: 226718; MSDS Number: 8026
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
API Gravity 32.7 °32.7 °
Brookfield Viscosity 11400 cP
@Temperature -40.0 °C
11400 cP
@Temperature -40.0 °F
Viscosity Measurement 184184Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 181 SUS181 SUS
Saybolt Viscosity at 210°F 51 SUS51 SUS
Kinematic Viscosity at 40°C (104°F) 36 cSt36 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 7.5 cSt7.5 cStASTM D445
 
Thermal PropertiesMetricEnglishComments
Pour Point -45.0 °C-49.0 °FASTM D97
Flash Point 228 °C442 °FASTM D92
 
Descriptive Properties
ColorRed
FZG Gear Wear Test, Failure Load Stage>12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCHEV051 / 74666

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.