MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Gougeon Brothers PRO-SET® XR29A~M2046 Fire Retardant Laminating Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Medium viscosity for good wet out of all synthetic composite fabrics and core materials.
Thixotroped to prevent drain out in heavy fabrics and on vertical surfaces.
High tack to help hold heavy fabric and core in place on vertical surfaces.
Fire retardant system (listed as XR02-099-29A) is accepted for compliance with Lloyd’s Register Rules and Regulations and with the International Convention for Safety of Life at Sea (SOLAS), 1974, as amended, for use on ships and offshore installations classed with Lloyd’s Register, and for use on ships and offshore installations when authorized by contracting governments to issue the relevant certificates, licenses, permits, etc.
Elevated temperature cure is required; thermal and mechanical properties suitable for composite components and high temperature tooling and molds.
Tg as high as 149° F (65°C) with proper post cure providing excellent temperature stability and great part cosmetics.

Information provided by Gougeon Brothers, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 115 cP115 cPhardener; ASTM D2196
 1000 cP1000 cPMixed; ASTM D2196
 1375 cP1375 cPresin; ASTM D2196
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 84
@Treatment Temp. 60.0 °C,
Time 28800 sec
84
@Treatment Temp. 140 °F,
Time 8.00 hour
RT Gelation; ASTM D2240
Tensile Strength 55.4 MPa
@Treatment Temp. 60.0 °C,
Time 28800 sec
8040 psi
@Treatment Temp. 140 °F,
Time 8.00 hour
RT Gelation; ASTM D638
Elongation at Break 3.9 %
@Treatment Temp. 60.0 °C,
Time 28800 sec
3.9 %
@Treatment Temp. 140 °F,
Time 8.00 hour
RT Gelation; ASTM D638
Tensile Modulus 2.85 GPa414 ksiRT Gelation; ASTM D638
Flexural Strength 96.5 MPa
@Treatment Temp. 60.0 °C,
Time 28800 sec
14000 psi
@Treatment Temp. 140 °F,
Time 8.00 hour
RT Gelation; ASTM D790
Flexural Modulus 2.94 GPa
@Treatment Temp. 60.0 °C,
Time 28800 sec
427 ksi
@Treatment Temp. 140 °F,
Time 8.00 hour
RT Gelation; ASTM D790
Compressive Yield Strength 71.91 MPa
@Treatment Temp. 60.0 °C,
Time 28800 sec
10430 psi
@Treatment Temp. 140 °F,
Time 8.00 hour
RT Gelation; ASTM D695
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 51.1 °C
@Treatment Temp. 60.0 °C,
Time 28800 sec
124 °F
@Treatment Temp. 140 °F,
Time 8.00 hour
RT Gelation; ASTM D648
Glass Transition Temp, Tg 65.0 °C149 °FASTM E1356
 52.8 °C
@Treatment Temp. 60.0 °C,
Time 28800 sec
127 °F
@Treatment Temp. 140 °F,
Time 8.00 hour
DSC Onset– 1st Heat, RT Gelation; ASTM E1356
 
Processing PropertiesMetricEnglishComments
Pot Life 225 - 275 min
@Load 0.100 kg
225 - 275 min
@Load 0.221 lb
ASTM D2471
Shelf Life 24.0 Month24.0 Monthhardener
 36.0 Month36.0 Monthresin
 
Descriptive Properties
Mix ratio100:26.0Weight, Resin: Hardener
 100:31.0Volume, Resin: Hardener
 3.23:1Volume, Resin: Hardener
 3.85:1Weight, Resin: Hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOUGP930 / 290773

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.