MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SEKISUI SPI KYDEX® 6565(d) Thermoplastic Sheet  (discontinued **)
Categories: Polymer; Thermoplastic

Material Notes: Decorative low heat release aviation sheet

KYDEX® 6565(d) is a proprietary, high performance, decorative thermoplastic sheet specifically formulated to meet the safety needs of the aviation industry

KYDEX® 6565(d) is a proprietary, high performance, decorative thermoplastic sheet that meets all fire retardancy requirements set forth in Federal Aviation Regulations 25.853 paragraphs (a) and (d) including low heat release (65/65) in the OSU rate of heat release test. Its excellent properties make it the ideal material to form two- and three-dimensional aircraft components.

Suggested Applications:

  • Seat parts
  • Window shades
  • Life vest shrouds
  • Passenger service units
  • Monitor shrouds
  • Bulkhead laminates
  • Armrests
  • Molding strips
  • Tray tables
  • Kick panels

Features:

  • Available in a wide range of thicknesses, enabling you to satisfy both the functional and aesthetic requirements of any aircraft interior.
  • Very resistant to a wide range of concentrate chemicals, and is therefore easy to clean with standard household cleaning agents excluding abrasive and concentrated products
  • Meets the stringent requirements of the FAR 25.853 (a) and (d) in all thicknesses and colors
  • Forms to deep draws with low forces when heated to the upper end of the proper forming temperature range
  • Crisp detail is achieved and rejects are minimized
  • Can be formed on all standard presses and cut on all standard die-cutting machines
  • Secondary operations include: machining, sawing, blanking, punching, etc. are easily performed

Values based upon 3.18 mm (0.125 in) sheet unless otherwise specified

Information provided by Sekisui Polymer Innovations

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.52 g/cc1.52 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 111111ASTM D785
Tensile Strength 43.0 MPa6240 psiASTM D638
Modulus of Elasticity 3.833 GPa555.9 ksiASTM D790
Flexural Strength 81.2 MPa11800 psiASTM D790
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 75.89 °C168.6 °FAnnealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Processing Temperature 163 - 199 °C325 - 390 °FForming Temperature
 
Descriptive Properties
Flammability<65 kW/m²FAR 25.853(d) Part IV; OSU Heat Release
 <65 kW-min/m²FAR 25.853(d) Part IV; OSU Heat Release
 Dmax<200FAR 25.853(d) Part V; NBS Smoke Density
 PassFAR 25.853(a)(i); Vertical Burn, 60 sec
 PassFAR 25.853(a)(ii); Vertical Burn, 12 sec

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SEKISUI SPI KYDEX® 410 ABS/PVC
SEKISUI SPI KYDEX® T Thermoplastic
SEKISUI SPI KYDEX® 430 ABS/PVC
SEKISUI SPI KYDEX® 510 Thermoplastic
SEKISUI SPI KYDEX® 6513 Thermoplastic

PSEKIS045 / 185870

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.