MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Eastman Cristal™ Renew EB062-99.8 Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Eastman Cristal™ Renew EB062-99.8 copolyester is a resin specifically developed for extrusion blown bottles where aesthetics such as high clarity and gloss, coupled with design flexibility, drive demand particularly in packaging for cosmetics and personal care. Compared to commonly used materials, Cristal Renew EB062-99.8 runs on most standard processing equipment. Extremely high melt strength makes the resin an excellent choice when manufacturing bottles. This product offers improved toughness, melt strength, chemical resistance, excellent color, and clarity in thick-walled applications. Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are produced with ISCC certified circular content by mass balance allocation. Cristal Renew EB062-99.8 is certified to NSF/ANSI Standard 51 for Food Equipment Materials. Cristal™ Renew EB062-99-8 is cleared for various food contact applications (including contact with most alcoholic beverages) by FCN No. 1234 as described in the Food and Drug Administration (FDA) Inventory of Effective Food Contact Substance Notifications and may be used in full compliance with the United States Federal Food and Drug, and Cosmetic Act, provided that it is used within the limitations set forth for FCN 1234.

Applications

  • Bottles-skin care pkg
  • Personal care & cosmetics packaging
  • Personal care bottles
  • Personal care packaging
  • Skin care packaging
Key Attributes
  • Easy to extrude, cut, print, and seal
  • Effective barrier properties
  • Excellent chemical resistance
  • Excellent clarity
  • Excellent colorability
  • Good impact strength
  • Good stiffness
  • High gloss appearance
  • Toughness

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/in³ASTM D792
Linear Mold Shrinkage 0.00300 cm/cm0.00300 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 105105ASTM D785
Tensile Strength at Break 48.0 MPa6960 psiASTM D638
Tensile Strength, Yield 47.0 MPa6820 psiASTM D638
Elongation at Break 300 %300 %ASTM D638
Elongation at Yield 5.00 %5.00 %ASTM D638
Tensile Modulus 1.90 GPa276 ksiASTM D638
Flexural Strength 65.0 MPa9430 psiASTM D790
Flexural Modulus 1.90 GPa276 ksiASTM D790
Izod Impact, Notched  0.630 J/cm
@Temperature -40.0 °C
1.18 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ASTM D4812
 NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
ASTM D4812
Puncture Energy  39.0 J
@Temperature -40.0 °C
28.8 ft-lb
@Temperature -40.0 °F
@ Max. Load; ASTM D3763
 41.0 J
@Temperature 0.000 °C
30.2 ft-lb
@Temperature 32.0 °F
@ Max. Load; ASTM D3763
 41.0 J
@Temperature 23.0 °C
30.2 ft-lb
@Temperature 73.4 °F
@ Max. Load; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 73.0 °C163 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 63.0 °C145 °FASTM D648
Vicat Softening Point 85.0 °C
@Load 1.00 kg
185 °F
@Load 2.20 lb
ASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 1.30 %1.30 %ASTM D1003
Gloss 143 %143 %60°; ASTM D2457
Transmission, Visible 87.0 %87.0 %Regular; ASTM D1003
 91.0 %91.0 %Total; ASTM D1003
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details
NSF YesYesSee notes for details
 
Descriptive Properties
Color-0.2a*, ASTM D2244
 0.6b*, ASTM D2244
 95L*, ASTM D2244

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM4073 / 323696

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.