MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for 5000 Series Aluminum Alloy
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 5000 Series Aluminum Alloy

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "5000 Series Aluminum Alloy". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.0160 - 2.84 g/ccAverage value: 1.82 g/cc Grade Count:297
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 28.0 - 185Average value: 84.9 Grade Count:93
Hardness, Knoop 68.0 - 150Average value: 98.9 Grade Count:56
Hardness, Rockwell A 35.4 - 46.8Average value: 39.2 Grade Count:18
Hardness, Rockwell B 49.0 - 75.0Average value: 57.1 Grade Count:21
Hardness, Vickers 46.0 - 137Average value: 87.6 Grade Count:56
Tensile Strength, Ultimate 110 - 590 MPaAverage value: 327 MPa Grade Count:115
Tensile Strength, Yield 40.0 - 540 MPaAverage value: 239 MPa Grade Count:115
Elongation at Break 0.500 - 35.0 %Average value: 11.9 % Grade Count:114
Modulus of Elasticity 68.9 - 73.0 GPaAverage value: 70.3 GPa Grade Count:104
Compressive Yield Strength 0.138 - 325 MPaAverage value: 15.9 MPa Grade Count:104
Compressive Modulus 0.0689 - 74.0 GPaAverage value: 13.4 GPa Grade Count:117
Notched Tensile Strength 207 - 331 MPaAverage value: 263 MPa Grade Count:8
Ultimate Bearing Strength 248 - 669 MPaAverage value: 492 MPa Grade Count:18
Bearing Yield Strength 83.0 - 476 MPaAverage value: 280 MPa Grade Count:18
Poissons Ratio 0.330 - 0.360Average value: 0.331 Grade Count:86
Fatigue Strength 82.7 - 365 MPaAverage value: 150 MPa Grade Count:41
Fracture Toughness 35.0 - 185 MPa-m½Average value: 117 MPa-m½ Grade Count:4
Machinability 10.0 - 50.0 %Average value: 34.0 % Grade Count:25
Shear Modulus 0.0469 - 72.4 GPaAverage value: 8.44 GPa Grade Count:179
Shear Strength 0.138 - 270 MPaAverage value: 31.1 MPa Grade Count:187
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000316 - 0.00000660 ohm-cmAverage value: 0.00000503 ohm-cm Grade Count:98
 
Thermal PropertiesOriginal ValueComments
CTE, linear 21.8 - 26.1 µm/m-°CAverage value: 24.2 µm/m-°C Grade Count:102
Specific Heat Capacity 0.857 - 0.960 J/g-°CAverage value: 0.897 J/g-°C Grade Count:86
Thermal Conductivity 105 - 205 W/m-KAverage value: 141 W/m-K Grade Count:102
Melting Point 568 - 657 °CAverage value: 623 °C Grade Count:82
Solidus 568 - 638 °CAverage value: 601 °C Grade Count:82
Liquidus 635 - 657 °CAverage value: 646 °C Grade Count:82
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 343 - 413 °CAverage value: 351 °C Grade Count:83
Hot-Working Temperature 260 - 510 °CAverage value: 387 °C Grade Count:83
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 88.2 - 99.8 %Average value: 95.5 % Grade Count:190
Beryllium, Be 0.000500 - 0.000800 %Average value: 0.000704 % Grade Count:28
Chromium, Cr 0.0100 - 0.500 %Average value: 0.175 % Grade Count:163
Copper, Cu 0.0300 - 0.800 %Average value: 0.145 % Grade Count:182
Cr + Mn 0.100 - 0.700 %Average value: 0.377 % Grade Count:10
Gallium, Ga 0.0300 - 0.0500 %Average value: 0.0340 % Grade Count:5
Iron, Fe 0.00800 - 1.20 %Average value: 0.424 % Grade Count:174
Lead, Pb 0.00300 - 1.80 %Average value: 0.534 % Grade Count:3
Magnesium, Mg 0.200 - 6.20 %Average value: 3.15 % Grade Count:190
Manganese, Mn 0.0100 - 1.80 %Average value: 0.410 % Grade Count:188
Nickel, Ni 0.0100 - 0.100 %Average value: 0.0440 % Grade Count:5
Scandium, Sc 0.0500 - 0.550 %Average value: 0.267 % Grade Count:3
Si+Fe 0.350 - 0.450 %Average value: 0.422 % Grade Count:16
Silicon, Si 0.0100 - 1.40 %Average value: 0.302 % Grade Count:174
Titanium, Ti 0.00800 - 0.200 %Average value: 0.135 % Grade Count:130
Vanadium, V 0.0500 %Average value: 0.0500 % Grade Count:14
Zinc, Zn 0.0100 - 2.80 %Average value: 0.260 % Grade Count:184
Zirconium, Zr 0.0500 - 0.300 %Average value: 0.158 % Grade Count:26
Zr+Ti 0.150 %Average value: 0.150 % Grade Count:8

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for 6000 Series Aluminum Alloy
Overview of materials for 3000 Series Aluminum Alloy
Overview of materials for 2000 Series Aluminum Alloy
Overview of materials for 7000 Series Aluminum Alloy
Overview of materials for 4000 Series Aluminum Alloy

M01044 / 81686

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.