SCG MDPE M545WC is a black medium density polyethylene compound for jacketing in power cable and communication cable applications. It contains well-dispersed carbon black to provide excellent weathering resistance and UV resistance. Applications: Jacketing of fiber optic cables, Jacketing of power cables. Features: Good surface appearance. Good mechanical properties. High extrusion speed. Information provided by SCG. |