Petrothene XL07438X01 is a colorable, non-halogenated, flame retardant compound crosslinkable via continuous vulcanization (C.V.). Petrothene XL07438X01 is selected by customers for use in 125 °C automotive wire & cable applications (ISO 6722). Status: Developmental Availability: North America Application: Wire & Cable Market: Wire & Cable Processing Method: Wire & Cable Information provided by LyondellBasell. |