Adflex KS 021 P is a reactor TPO (thermoplastic polyolefin) manufactured using Lyondell Basell’s proprietary Catalloy process technology. It is suitable for the extrusion and calendering of soft film and sheet, for the impact modification of polypropylene, as well as monolayer and multilayer air quenched blown films. It is also used by our customers as high cold impact resistance material for automotive color-matched interior trim applications. Key characteristics are flexibility and low temperature impact resistance. The grade is available in natural pellet form. Availability: Africa-Middle East; Asia-Pacific; Australia and New Zealand; North America; South & Central America Application: Automotive Flooring; Interior Automotive Applications; Polymer Modifier; Soft Profile & Sheets; Soft Touch Applications; Sports, Leisure & Toys; TPO Foils and Skins Market: Automotive; Compounding Processing Method: Blown Film; Calendaring; Compounding; Extrusion Blow Molding; Extrusion Flat-die; Thermoforming Attribute: Good Chemical Resistance; Good Flexibility; Good Shape Retention; High ESCR (Environmental Stress Cracking Resistance); Low Temperature Impact Resistance Automotive Specifications: FCA MS-DB590 CPN 3900; Ford WSS M4D777-A8; GM GMW15702-170020 Information provided by LyondellBasell. |