Description: Apcotex CB 620 is an APEO free Carboxylated Styrene-Butadiene Latex designed for its high mechanical stability makes it suitable for spraying (e.g. binding of non-woven fabrics). It can also be utilized for full bath impregnation of needle felt, and for application from a lick roller trough. It is manufactured by employing state-of-the-art emulsion polymerization technology ensuring product consistency. APCOTEX CB 620 is capable, without the addition of extra surface active agents, of being foamed up to very light cup weights. Advantages: - Self-crosslinking polymer for high efficient roofing felt application
- Cross-linked film is very hard and brittle at room temperature
- High resistance to acids and alkali
- Reinforcement of non-woven fabric for grinding application
- High efficient roofing felt application
Information provided by Apcotex Industries Limited |