MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Fujipoly Industries Sarcon® 20GSR Thin-Film GSR
Categories: Polymer; Film; Thermoset; Silicone

Material Notes: Sarcon GSR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.

Sarcon GSR is a composite of Heat Conductive Silicone Rubber and fiberglass.

Information provided by Fujipoly Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8585ASTM D2240
 858560°C for 500 hrs with 95% RH; ASTM D2240
 8888150°C for 1,000 hrs; ASTM D2240
Tensile Strength, Yield 30.0 MPa4350 psi150°C for 1,000 hrs; ASTM D1458
 70.0 MPa10200 psi
 80.0 MPa11600 psi60°C for 500 hrs with 95% RH
Elongation at Yield <= 3.0 %<= 3.0 %
 <= 3.0 %<= 3.0 %150°C for 1,000 hrs; ASTM D1458
 <= 3.0 %<= 3.0 %60°C for 500 hrs with 95% RH; ASTM D1458
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cm
 2.50e+15 ohm-cm2.50e+15 ohm-cm150°C for 1,000 hrs
 8.40e+16 ohm-cm8.40e+16 ohm-cm60°C for 500 hrs with 95% RH
Dielectric Constant  1.84
@Frequency 1000 Hz
1.84
@Frequency 1000 Hz
After 500 hrs at 60°C with 95% RH
 1.85
@Frequency 1e+6 Hz
1.85
@Frequency 1e+6 Hz
After 500 hrs at 60°C with 95% RH
 1.92
@Frequency 50 Hz
1.92
@Frequency 50 Hz
After 1000 hrs at 150°C
 1.92
@Frequency 1000 Hz
1.92
@Frequency 1000 Hz
After 1000 hrs at 150°C
 1.93
@Frequency 1e+6 Hz
1.93
@Frequency 1e+6 Hz
After 1000 hrs at 150°C
 2.09
@Frequency 50 Hz
2.09
@Frequency 50 Hz
After 500 hrs at 60°C with 95% RH
 2.6
@Frequency 1000 Hz
2.6
@Frequency 1000 Hz
 2.6
@Frequency 50 Hz
2.6
@Frequency 50 Hz
 2.6
@Frequency 1e+6 Hz
2.6
@Frequency 1e+6 Hz
Dielectric Strength 5.00 kV/mm127 kV/inAC 60 Hz
 6.00 kV/mm152 kV/inAC 60 Hz
 6.00 kV/mm152 kV/inAC 60 Hz
Dielectric Breakdown 3000 V3000 VWithstand Voltage [V/min]; AC 60 Hz
Dissipation Factor  0.00010
@Frequency 1000 Hz
0.00010
@Frequency 1000 Hz
After 500 hrs at 60°C with 95% RH
 0.00040
@Frequency 1e+6 Hz
0.00040
@Frequency 1e+6 Hz
After 500 hrs at 60°C with 95% RH
 0.00040
@Frequency 50 Hz
0.00040
@Frequency 50 Hz
After 500 hrs at 60°C with 95% RH
 0.00040
@Frequency 1e+6 Hz
0.00040
@Frequency 1e+6 Hz
 0.00050
@Frequency 1000 Hz
0.00050
@Frequency 1000 Hz
After 1000 hrs at 150°C
 0.00060
@Frequency 1e+6 Hz
0.00060
@Frequency 1e+6 Hz
After 1000 hrs at 150°C
 0.00070
@Frequency 1000 Hz
0.00070
@Frequency 1000 Hz
 0.0015
@Frequency 50 Hz
0.0015
@Frequency 50 Hz
After 1000 hrs at 150°C
 0.0026
@Frequency 50 Hz
0.0026
@Frequency 50 Hz
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 182 °C360 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
Flammability, UL94 V-0V-0
 
Descriptive Properties
ColorWhite
Thermal Impedance0.30°C/WFTM P-3010; ASTM D5470
Thermal Impedance AD Type0.64°C/WFTM P-3010; ASTM D5470

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik Vestamid® L1600 nf (dry properties) Nylon 12
DuPont™ Nomex® N196 Paper, 7 mil Nominal Thickness
DuPont™ Nomex® 419 Paper, 13 mil Nominal Thickness
DuPont™ Nomex® 411 Paper, 23 mil Nominal Thickness
DIAB Divinycell® F 50 Sandwich Core Material

PFUJIP35 / 39168

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.