MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Huntsman IROGRAN® A 98 E 4066 Polyester-Based TPU-High Performance Grade
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: Introduction: IROGRAN A 98 E 4066 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are very short cycle times and high dimensional stability.

Performance Features:

  • Short cycle times
  • High demolding stability
  • High production rates
  • High wear resistance
  • High hydrolysis resistance
Applications: For the production of technical parts, wheels and rollers, coupling halfs, sprocket wheels, buffers.

Information provided by Huntsman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/ccASTM D792
Linear Mold Shrinkage 0.0070 cm/cmASTM D995
Melt Index of Compound 15 g/10 min
@Load 21.6 kg,
Temperature 210 °C
cm3/10 min
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 97ASTM D2240
Hardness, Shore D 59ASTM D2240
Tensile Strength at Break 50.0 MPaDIN 53504
Elongation at Break 530 %DIN 53504
100% Modulus 0.0140 GPa
@Strain 100 %
DIN 53504
300% Modulus 0.0250 GPa
@Strain 300 %
DIN 53504
Rebound 30 %Bayshore; ASTM D2632
Tear Strength 770 pliASTM D624
Abrasion 30[mm3]; ISO 4649
Compression Set 30 %
@Temperature 23.0 °C,
Time 252000 sec
ASTM D395
 45 %
@Temperature 70.0 °C,
Time 86400 sec
ASTM D395
 
Processing PropertiesOriginal ValueComments
Feed Temperature 25.0 - 40.0 °CExtrusion
Front Barrel Temperature 165 - 190 °CExtrusion
Nozzle Temperature 170 - 200 °CExtrusion
 180 - 200 °CInjection Molding
Adapter Temperature 175 - 195 °CExtrusion
Die Temperature 175 - 200 °CExtrusion
Melt Temperature 170 - 195 °CInjection Molding
 185 - 200 °C
Mold Temperature 20.0 - 70.0 °CInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 98 E 4735 Polyester-Based TPU-Injection Extrusion Grade
Huntsman IROGRAN® A 85 E 4993 FCM Polyester-Based TPU-Injection Extrusion Grade
Covestro Desmopan® 1050D TPU
Barlog Plastics KEBAFLEX P D40.3 Polyester-Elastomer, Shore D40
Celanese Hytrel® 4056 TPC-ET

PHU9905 / 150365

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.