Market Segment: Compounding Suggested Uses Include Compounding Information provided by Sunoco Chemicals. Braskem acquired Sunoco Chemicals polypropylene product line in 2010. |
Highly Crystalline Homopolymer Phase, Very High Molecular Weight EPR Phase, Very High Flexural Modulus |