MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Osterman & Co Osterlene® LLB2019-SAH LLDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Product Description: LLB2019 has exceptional toughness and strength and ease of extrusion. Applications for LLB2019 include trash bags, liners, general packaging, industrial liners, heavy duty bags, stretch wrap, blend resin and industrial packaging.

Availability: North America
Additive: Antiblock: 6300 ppm; Slip: 1500 ppm
Features: Good Toughness; High Strength
Uses: Bags; Heavy-duty Bags; Industrial Applications; Liners; Packaging; Stretch Wrap
Processing Method: Extrusion

Information provided by Osterman & Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.919 g/cc0.0332 lb/in³ASTM D1505
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 6300 ppm6300 ppm
Slip Level 1500 ppm1500 ppm
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 10.3 MPa1500 psiASTM D882
Film Tensile Strength at Yield, TD 10.3 MPa1500 psiASTM D882
Film Elongation at Break, MD 660 %660 %ASTM D882
Film Elongation at Break, TD 700 %700 %ASTM D882
Secant Modulus, MD 0.170 GPa24.7 ksiASTM D790
Secant Modulus, TD 0.190 GPa27.6 ksiASTM D790
Elmendorf Tear Strength MD 110 g110 gASTM D1922
Elmendorf Tear Strength TD 330 g330 gASTM D1922
Dart Drop Test 100 g0.221 lbF50; ASTM D1709
Film Tensile Strength at Break, MD 31.7 MPa4600 psiASTM D882
Film Tensile Strength at Break, TD 24.8 MPa3600 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 14 %14 %ASTM D1003
Gloss 43 %43 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

POSTER101 / 267683

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.