MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Malvern Minerals Trikup® PF Silane Treated Aluminum Hydroxide
Categories: Ceramic; Oxide; Aluminum Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Trikup® is a custom, silane treated alumina trihydrate or aluminum hydroxide. ATH is the largest volume flame retardant in the world. Trikup® adds additional functionality through the use of epoxy, amino, vinyl and other silanes chosen to react with specific resin systems. Trikup® contributes brightness, opacity, gloss and smoothness to coatings. Additionally, Trikup® is exceptional for arc track resistance in PCBs and other composites. Additional fields include high power bushings and insulators. Typical Applications: Coatings, Silicone Rubber, Plastics, Wire & Cable, Adhesives, SMC/BMC, Composites

Information provided by Malvern Minerals Company.

Key Words: Al(OH)3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.42 g/cc
Bulk Density 41.0 lb/ft³
Brightness 93 %GE Brightness
Oil Absorption 41 %
Moisture Absorption at Equilibrium 0.30 %Free Moisture
Particle Size 3.0 - 4.0 µmAverage
pH 9.0
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 2.5 - 3.5
 
Optical PropertiesOriginal ValueComments
Refractive Index 2.40
 
Component Elements PropertiesOriginal ValueComments
Al2O3 64.9 %
Fe2O3 0.0090 %
Loss on Ignition(%) 34.6 %
Other 0.25 %total soda
SiO2 0.010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bakelite® PF 31 Phenolic Formaldehyde Resin, UL Listed
CeramTec ATZ Alumina Toughened Zirconia, Dental Grade
Cancarb Thermax® Powder N908 Stainless Medium Carbon Black
Bohler-Uddeholm UDDEHOLM MIRRAX ESR Plastic Mold Steel
Bakelite® UP 802 Unsaturated Polyester Resin, High Surface Quality, Low Shrinkage, High Arc Resistance

CMALV931 / 149111

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.