MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Redwood Plastics Redco™ SURE GLIDE UHMW
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: Redco™ Sure Glide has remarkable durability with significant abrasion resistance and dimensional stability. It has a low coefficient-of-friction with a surface slickness that rivals PTFE, while also having good tensile strength, impact resistance and load-bearing properties. Redco™ Sure Glide excels in demanding applications such as guides for heavy-duty conveyor chains, wear strips, and anywhere else a non-stick, extended-wear, liner surface is desired to reduce clogging and bridging in hoppers and chutes.

Standard Color: Dark Grey

Typical Applications: Aggregate chutes, bin liners, hopper liners, flume liners, belt scrapers, skirt boards, chutes, conveyors, silos, cyclones, spoon liners, bunkers, wear strips, feeder liners, etc.

Information provided by Redwood Plastics and Rubber

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.932 - 0.960 g/ccASTM D 792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 62 - 67ASTM D 2240
Tensile Strength 2700 - 2900 psiASTM D638
Elongation at Break >= 300 %ASTM D 638
Izod Impact, Notched NBASTM D 256
Coefficient of Friction, Dynamic 0.070 - 0.10
Coefficient of Friction, Static 0.12 - 0.15
 
Thermal PropertiesOriginal ValueComments
CTE, linear 100 µm/m-°CASTM D 696
Melting Point 275 - 280 °FASTM 789
Maximum Service Temperature, Air 180 °FContinuous

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PREDW018 / 296584

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.