MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Amodel® A-1340 HS Polyphthalamide (PPA) Resin, 40% Mineral/Glass Reinforced, Dry as Molded  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), Mineral Filled

Material Notes: AMODEL® A-1340 HS is a 40% mineral/glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, high tensile strength and low warpage. Excellent dimensional stability and low moisture absorption are also characteristics of this resin.

AMODEL A-1340 HS resin can be easily processed using conventional equipment and methods.

Information provided by Solvay Advanced Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.48 g/ccISO 1183A
 1.54 g/ccASTM D792
Moisture Absorption at Equilibrium 0.16 %24 hours; ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 125ASTM D785
Tensile Strength, Yield 151 MPaISO 527
 174 MPaASTM D638
 46.0 MPa
@Temperature 175 °C
ISO 527
 49.0 MPa
@Temperature 150 °C
ISO 527
 97.0 MPa
@Temperature 100 °C
ISO 527
Elongation at Break 1.8 %ISO 527
 2.3 %
@Temperature 100 °C
ISO 527
 7.0 %
@Temperature 175 °C
ISO 527
 7.4 %
@Temperature 150 °C
ISO 527
Elongation at Yield 2.2 %ASTM D638
Tensile Modulus 11.0 GPaASTM D638
 11.6 GPaISO 527
 2.70 GPa
@Temperature 175 °C
ISO 527
 3.10 GPa
@Temperature 150 °C
ISO 527
 8.00 GPa
@Temperature 100 °C
ISO 527
Flexural Strength 234 MPaISO 178
 263 MPaASTM D790
 55.0 MPa
@Temperature 175 °C
ISO 178
 63.0 MPa
@Temperature 150 °C
ISO 178
 155 MPa
@Temperature 100 °C
ISO 178
Flexural Modulus 9.10 GPaISO 178
 10.6 GPaASTM D790
 2.30 GPa
@Temperature 175 °C
ISO 178
 2.50 GPa
@Temperature 150 °C
ISO 178
 6.80 GPa
@Temperature 100 °C
ISO 178
Poissons Ratio 0.38
Shear Modulus 3.99 - 4.20 GPaCalculated
Shear Strength 91.0 MPaASTM D732
Izod Impact, Notched 45.0 J/mASTM D256
Izod Impact, Notched (ISO) 4.00 kJ/m²ISO 180/1A
Izod Impact, Unnotched (ISO) 31.0 kJ/m²ISO 180/1U
Charpy Impact Unnotched 4.50 J/cm²ISO 179/1eU
Charpy Impact, Notched 0.330 J/cm²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+15 ohm-cmASTM D257
 1.00e+16 ohm-cmASTM D257
Dielectric Constant 4.3
@Frequency 1e+6 Hz
ASTM D150
 4.5
@Frequency 100 Hz
ASTM D150
Dissipation Factor 0.0050
@Frequency 100 Hz
ASTM D150
 0.017
@Frequency 1e+6 Hz
ASTM D150
High Voltage Arc Resistance to Ignition (HVAR) 150 secASTM D495
Comparative Tracking Index 550 VASTM D3638
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 19.0 µm/m-°C
@Temperature 160 - 250 °C
 29.0 µm/m-°C
@Temperature 0.000 - 100 °C
CTE, linear, Transverse to Flow 46.0 µm/m-°C
@Temperature 0.000 - 100 °C
 92.0 µm/m-°C
@Temperature 160 - 250 °C
Melting Point 313 °CISO 11357-3
 313 °CASTM D3418
Maximum Service Temperature, Air 130 °C20000 hours, Continuous; ASTM D3045
 150 °C5000 hours, Continuous; ASTM D3045
Deflection Temperature at 0.46 MPa (66 psi) 290 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 262 °CISO 75Af
 275 °CASTM D648
Flammability, UL94 HB

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOLVT62 / 21358

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.