MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Radici RADILON® MIXLOY S 32HSA20K 100 NT PA6/ABS Blend, Heat Stabilized, Conditioned
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend

Material Notes: Description: PA6/ABS blend, medium viscosity extrusion grade. Heat stabilized. Natural color. Suitable for parts requiring low moisture absorption and high dimensional stability. Also apt for 3D printing

Processing: 3D Printing, Profile Extrusion, Other Extrusion

Delivery Form: Granules

Additives: Lubricants, Release agent

Special Characteristics: Heat stabilized or stable to heat, Amorphous, Improved Dimensional Stability, High Surface Aspect, Low Moisture Absorption

Industries: Automotive, Consumer Industry Goods, Transportation

Regional Availability: North America, Europe, Asia Pacific, South and Central America, Near East/Africa

Information provided by Radici Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³ISO 1183
Water Absorption 6.4 %
@Thickness 2.00 mm
6.4 %
@Thickness 0.0787 in
Immersion at 23°C; ISO 62
Moisture Absorption 2.00 %
@Thickness 2.00 mm
2.00 %
@Thickness 0.0787 in
50% RH; ISO 62
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 260 °C500 °F
Middle Barrel Temperature 260 °C500 °FCenter Rear
 265 °C509 °FCenter Front
Front Barrel Temperature 270 °C518 °F
Melt Temperature 275 °C527 °F
Head Temperature 275 °C527 °FHead and Die

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRADICI104 / 313605

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.