A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range of applications. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding, extrusion or blow molding. It is polyolefin based and completely recyclable. Key Features: - UL listed: file #QMFZ2.E80017, Plastics - Component; file #QMFZ8.E80017, Plastics Certified For Canada - Component.
- Although not NSF certified, this product has a Material Supplier Form on file with NSF to facilitate its evaluation for use in applications requiring NSF certification.
- Recommended for applications requiring excellent flex fatigue resistance.
- Excellent ozone resistance.
- EU and China RoHS compliant.
Applications: - Automotive-Plugs, Bumpers, Grommets, Clips, Seals and Gaskets
- Industrial-Seals and Gaskets
- Soft Touch Grips
- Tubing
Uses:- Appliance Components
- Automotive Applications
- Automotive Under the Hood
- Consumer Applications
- Diaphrams
- Electrical Parts
- Gaskets
- Seals
- Tubing
Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical |
EU 203/11/EC; RoHS Compliant; UL JMLU2; UL QMFZ2; UL QMFZ8 |