Components: Polyamide based filament filled with 30% glass fibers for Fused Filament Fabrication. Product Description: Ultrafuse® PA6 GF30 is polyamide, reinforced with 30% glass fiber content. The fibers in this material are specially designed for 3D-printing filaments and are compatible with a wide range of FFF 3D-printers. The extreme stiffness and strength make this material highly suitable for demanding applications. Ultrafuse® PA6 GF30 has a good chemical and wear resistance. With its excellent layer adhesion and the low warping, it is designed to be easy to use and suitable for a wide range of applications. Information provided by BASF |