MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Aperam Superimphy® NY811 (800HT) Bar-Corrosion application
Categories: Metal; Ferrous Metal

Material Notes: NY811 (800HT) is a Fe-Ni-Cr (Ti+Al) alloy widely used for construction of equipment requiring corrosion resistance, heat resistance and strength. Phy800 is mainly used in general corrosion resistance to many aqueous environment. At elevated temperatures it offers good resistance to oxidation, carburization, and sulfidation along with rupture and creep strength. For applications requiring greater resistance to stress rupture and creep, especially for T > 816°C, Phy 810 or 811 are used.

Applications:

  • Chemicals Industries (Nitric acid)
  • Petrochemical processing
  • Heat exchanger and piping system
  • Nuclear power plant (steam generator tubing)
  • Sheathing of electric heating elements
Standards related to these applications: ASTM B408 or B564; AMS 5766

Information provided by Aperam

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.15 - 0.60 %0.15 - 0.60 %
Carbon, C 0.060 - 0.10 %0.060 - 0.10 %
Chromium, Cr 19 - 23 %19 - 23 %
Iron, Fe >= 39.5 %>= 39.5 %
Nickel, Ni 30 - 35 %30 - 35 %
Titanium, Ti 0.15 - 0.60 %0.15 - 0.60 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NPERA028 / 194817

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.