MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Gichem GIPLENE CVX45/CV0 Polypropylene - Flame Retardant  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Flame Retardant

Material Notes: PP 20% glass fiber, self-extinguishing, class V0. Medium injection speed.

Information provided by GICHEM Gruppo Industriale Chimico

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³ASTM D792
Water Absorption 0.020 %0.020 %ASTM D570
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm0.0050 - 0.0080 in/inASTM D955
Melt Flow 5.0 g/10 min5.0 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 55.0 MPa7980 psiASTM D638
Elongation at Yield 3.0 %3.0 %ASTM D638
Flexural Modulus 5.00 GPa725 ksiASTM D790
Izod Impact, Notched 0.500 J/cm0.937 ft-lb/inASTM D256
 0.400 J/cm
@Temperature 0.000 °C
0.749 ft-lb/in
@Temperature 32.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 145 °C293 °FASTM D648
Vicat Softening Point 125 °C257 °FASTM D1525/A
Flammability, UL94  V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
Flammability Test 125125[°C] Bilia; IEC 331
Oxygen Index 27 %27 %ASTM D2863
Glow Wire Test 960 °C1760 °FIEC 695-2-1
 
Processing PropertiesMetricEnglishComments
Middle Barrel Temperature 180 - 200 °C356 - 392 °F
Mold Temperature 60.0 °C140 °F
Drying Temperature 60.0 °C140 °F2 hours

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex HFFR 2006 Polyolefin, Halogen Free
Teknor Apex HFFR 2005PC Polyolefin, Halogen Free
Teknor Apex HFFR 2003PC Polyolefin, Halogen Free
Teknor Apex HFFR 2002 Polyolefin, Halogen Free
RTP Company RTP 150 Polypropylene (PP), Flame Retardant - UL94 V-0

PGICH23 / 41840

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.