MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Sika Sikasil® 728 NS Non-sag, ultra low modulus, highway/parking garage, neutral cure silicone sealant
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: Sikasil 728 NS is a high performance, non-sag. one-component , ultra low modulus elastomeric, neutral cure silicone sealant. Meets the requirements of ASTM D-5893: ASTM C-920, Type S, Grade NS, Class 100/50, Use NT, T, M, G, A, O with ultra low Shore Hardness: TT-S-00230C, Type II, Class A; Class A.

Where to Use: Construction Application:

  • Highway joints
  • Bridges
  • Stadiums
  • Parking garages
  • Plaza decks
  • Driveways
  • Decks
  • Expansion joints
  • Saw cut joints Substrate:
    • Concrete, steel, glass, aluminum, ceramic, masonry, brick, stone and granite.
    Advantages:
    • Durable
    • Ideal for cold climates
    • Excellent flexibility for extreme high and low temperature conditions
    • Excellent flexibility for dynamic joint movement
    • Bonds to most substrates without priming; best performance obtained in horizontal joints when primed
    • Ready to use, labor cost reduction
    • Non sag, excellent for vertical joints
    • All season ease of application
    • Excellent for use on all types of concrete joints
    • Jet fuel resistant
    • Resistant to road salts

    Information provided by Sika Corporation.

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Volatile Organic Compounds (VOC) Content 21 g/l1.64% by wt
     
    Mechanical PropertiesOriginal ValueComments
    Hardness, Shore A 5.0 - 10ASTM C-661 & ASTM D-2240
    Hardness, Shore OO 50ASTM C-661 & ASTM D-2240
    Tensile Strength 175 psiASTM D412
    Tensile Stress at Strain 35.0 psi
    @Strain 100 %
    ASTM D412
    Elongation at Break 1000 %ASTM D412
    Peel Strength 40.0 pliASTM C794
     
    Thermal PropertiesOriginal ValueComments
    Maximum Service Temperature, Air 350 °F
    Minimum Service Temperature, Air -80.0 °F
     
    Processing PropertiesOriginal ValueComments
    Cure Time 15.0 - 25.0 minSkin-over Time
     24.0 hour
    @Thickness 1.59 mm
    Tack-Free Time 30.0 - 40.0 minASTM C679
    Shelf Life 12.0 Month
    @Temperature <=32.0 °C
    in original unopened cartridge
     
    Descriptive Properties
    ColorLimestone and Charcoal Gray

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    PSIKA950 / 209857

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.