MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Corning Pyroceram® Code 9606 Glass Ceramic
Categories: Ceramic; Glass; Glass Ceramic

Material Notes: High strength, high elastic modulus, and uniform dielectric properties. Pyroceram® can be manufactured in ogival (pointed arch) shapes, hemispheres, pressware sheets, and various machined shapes. Uses include:
  • Tactical Missile Nose Cones
  • Antenna Windows
  • Radomes
  • Solid Wave Guides
  • Hydrospace Systems

Information provided by Corning Incorporated.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.60 g/cc
Water Absorption <= 0.01 %
Porosity 0.0 %
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 120 GPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.70 µm/m-°C
@Temperature 20.0 - 320 °C
Specific Heat Capacity 0.974 J/g-°C
Thermal Conductivity 0.00810 cal cm/sec-cm²-°C
@Temperature 20.0 - 800 °C
Softening Point 1350 °C
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 0.0 %opaque
 
Descriptive Properties
ColorLight Gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borosilicate Glass
Cordierite, 2MgO-2Al2O3-5SiO2
Corning Pyrex® 7740 Borosilicate Glass Sheet
Dicor Castable Fluormica Glass-Ceramic
420 Stainless Steel

CCORNG15 / 178183

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.