MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ICE Steatite L-4
Categories: Ceramic; Oxide; Magnesium Oxide; Silicon Oxide

Material Notes: Data provided by the manufacturer, International Ceramic Engineering.

Key Words: International Ceramic Engineering soapstone, talc, H2Mg3(SiO3)4
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 0.00 - 0.030 %0.00 - 0.030 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 7.57.5
Tensile Strength, Ultimate 70.0 MPa10200 psi
Flexural Strength 100 MPa14500 psi
Compressive Strength 550 MPa79800 psi
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 5.8
@Frequency 1e+6 Hz
5.8
@Frequency 1e+6 Hz
Dielectric Strength 9.40 kV/mm239 kV/in
Dielectric Loss Index 0.014
@Frequency 1e+6 Hz
0.014
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.30 µm/m-°C
@Temperature 25.0 - 600 °C
4.61 µin/in-°F
@Temperature 77.0 - 1110 °F
Maximum Service Temperature, Air 1425 °C2597 °F
 
Descriptive Properties
ColorCream

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Frequentite 1000 Steatite
GBC L3 Steatite
ICE Steatite L-5
China-Yixing Longly Refractories Steatite Ceramics (High Frequency Porcelain)
CeramTec Frequenta® Steatite

CI008 / 1384

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.