MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Dow ELVALOY™ 4170P Polymer Modifier
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: ELVALOY™ 4170P is an ethylene terpolymer, used as an Impact Modifier for a variety of polymers. It is a low volatile version of ELVALOY™ 4170.
Uses: Polymer Modifier
Composition: Ethylene Terpolymer
Characteristics/Benefits: Impact modifier/compatibilzer for PET and PBT
Applications: When used in a CPET tray formulation, ELVALOY™ 4170P provides both toughening and increases the melt strength of the PET.

Availability: Africa & Middle East; Asia Pacific; Latin America; Europe; North America

Additive: Impact Modifier

Processing Method: Extrusion

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/ccISO 1183
 0.942 g/ccASTM D792
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 8.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Thermal PropertiesOriginal ValueComments
Melting Point 162 °FPeak; ASTM D3418
 162 °FISO 3146

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWF505 / 311198

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.