MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Evonik TEGOMER® P 161 Dispersing Aid
Categories: Other Engineering Material

Material Notes: Product description: TEGOMER® P 161 is a siloxane polyolefine compound delivered in pelletized form.

Application: TEGOMER® P 161 serves as dispersing aid for highly loaded compounds containing 40 to 80 % mineral fillers like talc, calcium, CaCO3 and Sb2O3. In the processing the use of TEGOMER® P 161 leads to a reduction of amperage draw and a slightly increased MFI of the compound. Due to the excellent dispersing properties of TEGOMER® P 161 the bulk characteristics are improved by:

  • higher impact strength
  • higher tensile strength
Furthermore TEGOMER® P 161 improves the production of blown film or injection molded parts with thin walls by:
  • avoiding of film fracture
  • superior speck evaluation
  • improved film quality

    TEGOMER® P 161 enhances the dispersion of compounds filled with 50 to 70 % TiO2 and is used successful for coloration of films, especially if color pigments are used in combination. Stripe formation or discoloration is avoided.

    Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.400 - 0.600 g/cc
 
Thermal PropertiesOriginal ValueComments
Melting Point >= 100 °C
 
Descriptive Properties
Appearancewhite pellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Silon Taboradd 13-08480 Processing Aid Masterbatch
Overview of materials for Low Density Polyethylene (LDPE), Wire/Cable Grade
Overview of materials for Low Density Polyethylene (LDPE), Extrusion Grade
Mapal Plastics Maplon PAPER MATCH Polypropylene Sheet
Karina 1000/5035-IE MBPEB White Color Concentrate

PEVONIL591 / 196795

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.