MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Denka TX-100S Transparent Resin Polymer (MS resin) Methyl Methacrylate Styrene
Categories: Polymer; Thermoplastic

Material Notes: "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a good balance of transparency, strength and fluidity (methyl methacrylate butadiene styrene), "TE Series/CL Series," transparent ABS resins with excellent color attributes and tensile strength are available (among others).

Applications

TX is used for:

  • flat display substrates
  • optical components
  • miscellaneous goods.
TP/TH are used for:
  • food package sheeting as well as in manufacturing
  • electronic equipment and components
  • miscellaneous goods
TE/CL are for:
  • electronic equipment and components
  • information equipment components
  • AV equipment, etc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.12 g/cc1.12 g/ccASTM D792
Density 1.127 g/cc0.04072 lb/in³ISO 1183
Melt Flow  1.9 g/10 min
@Load 5.00 kg,
Temperature 200 °C
1.9 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ISO 1133
 26 g/10 min
@Load 10.0 kg,
Temperature 220 °C
26 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8686ISO 2039-2
Tensile Strength at Break 70.0 MPa10200 psi5mm/min; ASTM D638
 73.0 MPa10600 psi5mm/min; ISO 527-2
Elongation at Break 6.0 %6.0 %5mm/min; ISO 527-2
Flexural Strength 107 MPa15500 psi2mm/min; ASTM D790
 111 MPa16100 psiISO 178
Flexural Modulus 3.32 GPa482 ksi2mm/min; ISO 178
 3.35 GPa486 ksi2mm/min; ASTM D790
Izod Impact Resistance 1.80 J/cm²8.57 ft-lb/in²
Charpy Impact, Notched 0.200 J/cm²0.952 ft-lb/in²ISO 179-2
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 77.0 °C171 °FISO 75-2
 87.0 °C189 °FASTM D648
Vicat Softening Point 100 °C212 °F50N; ISO 306
Flammability, UL94 HBHB
 
Optical PropertiesMetricEnglishComments
Haze 0.20 %
@Thickness 2.00 mm
0.20 %
@Thickness 0.0787 in
ISO 14782
Transmission, Visible 92 %
@Thickness 2.00 mm
92 %
@Thickness 0.0787 in
ISO 13468-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Denka TX-400S Transparent Resin Polymer (MS resin) Methyl Methacrylate Styrene
Ashley Polymers Ashlene® D870, D870L, Transparent Amorphous Nylon
INEOS Styrolution NAS® 90 Styrene Methyl Methacrylate (SMMA)
A. Schulman Diamond SAN 267 Styrene Acrylonitrile, Transparent Engineering Thermoplastic
Evonik Trogamid® CX7323 Transparent Nylon

PDENK010 / 29674

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.