MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Armacell Okabell® ASD Aluminized Steel
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Description: High integrity aluminized steel jacketing with hot-dip aluminum-silicon alloy coating on both sides.

Special Features: Excellent corrosion resistance, far superior to pure zinc and zinc-aluminum alloy coatings. The hot-dip aluminum-silicon alloy coating protects the steel substrate by forming an inert barrier. Therefore cut edges or areas that may be damaged at a later date may corrode slightly but stabilize in short time, reducing the risk of further corrosion. This process is unlike zinc coatings which protect the steel substrate through sacrificial oxidation. Zinc salts formed during the coating process are constantly washed away, leaving the steel exposed and at risk of corrosive attack.

Application: Low cost alternative to stainless steel and aluminum.

Information provided by Armacell®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Taber Abrasion, mg/1000 Cycles 20[g], 250 rev, CS 10 wheels; EN 13523-16
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 120 °C
Minimum Service Temperature, Air -50.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ArcelorMittal AS60 Aluminized steel
ASTM A463 Aluminum-Coated Steel, Type I, Drawing Quality, Special Killed
ArcelorMittal AS100 Aluminized steel
ArcelorMittal AS80 Aluminized steel
ArcelorMittal 57+AS Aluminized steel

PARMD171 / 186782

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.